| Brand Name |
MgO |
SiO2 |
Fe2O3 |
Setting |
Grading |
Sintering |
Application |
Application Area |
| |
(%) |
(%) |
(%) |
|
(mm) |
Temp. ('C) |
Temp. ('C) |
|
| |
Min. |
Max. |
Max |
|
|
Min. |
Max. |
|
| SR M-95 |
94 |
1.5 |
- |
Chemical |
0-5 |
1550 |
1750 |
Tap Hole of BOF |
| SR Hearth-1 |
85 |
5 |
6 |
Chemical |
0-8 |
1400 |
1750 |
Dry Ramming Mass for EAF bottom |
| SR Hearth-II |
80 |
1.5 |
6 |
Chemical |
0-8 |
1400 |
1750 |
Dry Ramming Mass for EAF bottom |
| SR M-90 |
90 |
5 |
- |
Chemical |
0-5 |
1550 |
1750 |
Dry Ramming Mass for EAF & other application |
| SR M-84 |
83 |
8.5 |
- |
Chemical |
0-5 |
1550 |
1750 |
Wet Ramming Mass for EAF |
| SR M-84(SPL) |
83 |
7.5 |
- |
do |
0-5 |
1550 |
1750 |
do |
| SR-L(C)X |
70 |
Cr2O3:8 |
- |
do |
0-5 |
800 |
1750 |
Dry Ramming mass for |
| |
|
(Min.) |
|
|
|
|
|
Induction furnace melting |
| |
|
|
|
|
|
|
|
mild steel & alloy steel |
| SR coat-M |
88 |
- |
- |
do |
0-0-5 |
- |
- |
Protective coating of coils of |
| |
|
|
|
|
|
|
|
high frequency induction furnace |